Reflective powder using method

Reflective powder using method:


Water-based screen printing (1) :

The reflective powder can be directly adding into the water-based glue paste.Stir uniform.(can adding the fertilizer appropriately to strengthen the fastness).Then can stamp and print.

 

Water-based screen printing (2):

Directly adding into the transparent pulp.Stir uniform.(can adding the fertilizer appropriately to strengthen the fastness).Then can stamp and print.

 

Reflective powder oily screen printing (1):

Directly adding into the light oil.Stir uniform.(can adding the fertilizer appropriately to strengthen the fastness).Then can stamp and print.

 

Reflective powder oily screen printing  (2):

Directly adding into the ink,and make the reflective ink.Screen printing or brush on the fabric or other items.The using operation is convenient and easy to grasp.The adding amount should according to the reflective brightness.

 

The oily screen printing  (3):

First print the stamp pulp---reflective pulp ---drying curing.Reflective slurry preparation:according to the dosage,after weighing the reflective powder,using the solvent (cyclohexanone) tune into a paste,then adding into the the transparent stamp pulp.Stir uniform.When printing,the printing rubber thickness must be thin.30 microns - 50 microns will be the best.In order to ensure it can be exposed for half on the surface,then ca get the reflective effect.Can also according to the purpose,using the thicknesses particle size,will obtain all kinds of reflective effects.(the particle size be more different ,the reflective effect will be better)

 

Reflective powder spraying  :

Using the reflective base coating to spray.Until the reflective base coating get dry,then print the finish coating.If its the construction of the cement surface.Suggest for print two layers of reflective base coating.The effect will be much better.

Recommended to use the W - 71 type spray gun(nozzle 1.50 mm).The base coating should use the spray gun which pressure be around 2.0 Kg/cm2,the finish coating should use the spray gun which pressure be around 3.0kg/cm2 .When construction,the spray gun and the surface need to keep a distance of 18 cm,spray gun angle 45 °.The spray paint film layer should be uniform and thin,that will obtain the better effect. For the unknown substrate,should trial for a small part first.Do not construction in rainy fog or snow such bad days,it will affect the fastness.

 